$100.00
Annealing CNT yarn
If you would like any of our Galvorn materials to be annealed at high temperature to remove any trace impurities, add this service to your order and we will bake the Galvorn material in a furnace at 500 Celsius in a nitrogen environment for 4 hours. This will not affect the strength of the material, but may increase the electrical resistance by as much as a factor of 4.